Samples of cryogels based on aqueous solutions of polyvinyl alcohol were investigated. The molecular weights of cryogel samples varied from 25 × 103 to 60 × 103. It has been found out that the ultimate strength of dry briquettes increases from 1.2 to 3.7 MPa with an increase in the polymer molecular weight. The resulted briquettes can be used, for example, as a proper domestic or industrial fuel.

Full Text

Restricted Access

About the authors

M. S. Fufaeva

Institute of Petroleum Chemistry, Siberian Branch of the Russian Academy of Sciences

Author for correspondence.
Email: maria81@ipc.tsc.ru
Russian Federation, Tomsk

V. N. Manzhay

the Russian Academy of Sciences

Email: mang@ipc.tsc.ru
Russian Federation, Tomsk

References

  1. Лозинский В.И. // Успехи химии. 1998. Т. 67. № 7. С. 641. [Russian Chemical Reviews, 1998, vol. 67, no. 7, p. 651. https://doi.org/10.1070/RC1998v067n07ABEH000399].
  2. Hassan C.M., Peppas N.A. // Adv. Polym. Sci. 2000. V. 53. Р. 37.
  3. Ушаков С.Н. Поливиниловый спирт и его производные. М.: Изд-во АН СССР, 1960. Т. 2. 868 с.
  4. Николаев А.Ф., Орхименко Г.И. Водорастворимые полимеры. Л.: Химия, 1979. 144 с.
  5. Малкин А.Я. Основы реологии. С-Пб: Профессия, 2018. С. 474.
  6. Manzhai V.N., Fufaeva M.S., Kashlach E.S. // Chinese J. Polym. Sci. 2023. V. 41. P. 442. https://doi.org/10.1007/s10118-022-2889-8

Supplementary files

Supplementary Files
Action
1. JATS XML
2. Fig. 1. Dependence of dynamic viscosity of PVA solutions (C = 100 kg/m3) on shear rate at 20°C, where molecular mass of polymer samples: (1) 25,000 (degree of hydrolysis 88%); (2) 25,000; (3) 46,000; (4) 54,000; (5) 59,000

Download (76KB)
3. Fig. 2. Rheological unit constructed on the basis of Maxwell's model: (a) mock-up of the unit: (1) scale, (2) micrometer head, (3) micrometer, (4) micrometer stem, (5) cryogel sample, (6) tripod; (b) laboratory unit

Download (79KB)
4. Fig. 3. Dependence of instantaneous modulus of elasticity of cryogels formed from PVA samples of different molecular weight on polymer concentration, at relative deformation of samples (ε = 0.08)

Download (54KB)
5. Fig. 4. Cryogel: (a) microfragment of cryogel volume, polymer frame of which is formed from low molecular weight samples of polyvinyl alcohol; (b) microfragment of cryogel volume, polymer frame of which is formed from high molecular weight samples of PVA

Download (115KB)

Copyright (c) 2024 Russian Academy of Sciences